A283 Gr. C STEEL PLATE
2013年7月15日 by admin
A283 Gr. C STEEL PLATE
Gangsteel Grade : | ASTM A283 GRADE C |
Specification (mm) | THK: 6 to 300, Width: 1500 to 4050, Length: 3000 to 27000 |
Standard: | ASTM A283 Standard Specification is for Low and Intermediate Tensile Strength Carbon Steel Plates |
ABS, DNV, GL, CCS, LR , RINA, KR, TUV, CE | |
Classification: | Low and Intermediate Tensile Strength Carbon Steel Plates |
Supplementary Technology: HIC Test | NACE MR0175 | Z15 | Z25 | Z35| S2 | S3 | S5 | S6 | S8 | S15 | S97 | S97.1 |
A283 Grade C Chemical Composition | ||||||
Grade | The Element Max (%) | |||||
C | Si | Mn | P | S | Cu (min) | |
A283 GR.C | 0.24 | 0.15-0.40 | 0.90 | 0.035 | 0.04 | 0.20 |
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Grade | A283 Grade C Mechanical Property | |||
Thickness | Yield | Tensile | Elongation | |
A283 GR.C | mm | Min Mpa | Mpa | Min % |
t≦50 | 205 | 380-515 | 25 | |
50<t≦200 | 205 | 380-515 | 22 |
Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
Equivalent steel grade of A283 Grade C | ||||||||
| | | | | | | | U.K |
S185,Fe 310-0 | A 320 | St 33 | A 33 | Fe 320 | SS13,00,00 | | SS 330 | |
Related Grade: A283 Grade B | A283 Grade C |A283 Grade D | A283 GR.A
Henan Gang Iron and Steel Co. Ltd( Gangsteel) is specialized in low alloy high strength structural steel, mainly dealing with specification standard plates in EN 10025-2, EN 10025-3, EN 10025-4, EN 10025-6, ASTM A633, ASTM A573, ASTM A572, DIN 17100, JIS G3106, ASTM A709, ASTM A283, ASTM A529, ASTM A656, EN 10225, ISO 630, NFA 35-501, and so on, the thickness up to 300mm.
To find out more about A283 Gr. C or other low alloy high strength steel, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.